HFA471 is non TBBA and environmental ABS resin. It has good heat stability and high fall ball impact. HFA471 is mainly used in computer monitor?printer?copier?TV shell?plug connecter requiring flame class, etc.Information provided by Shanghai Kumho Sunny Plastics co, Ltd |