MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Constellium Planoxal® 60 Aluminum plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly used for medium stressed machine elements which are subject to heavy machining, particularly for parts that require anodizing. Applications include packaging, printing and handling machines.

Information provided by manufacturer

Key Words: EN AW-6082; Al Si1MgMn
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 105
@Thickness 4.99 - 20.0 mm
 105
@Thickness 20.0 - 80.0 mm
Tensile Strength >= 295 MPa
@Thickness 12.5 - 60.0 mm
Temper T651; Standard EN 485-2
 >= 295 MPa
@Thickness 60.0 - 80.0 mm
Temper T651; Standard EN 485-2
 >= 300 MPa
@Thickness 6.00 - 12.0 mm
Temper T651; Standard EN 485-2
 >= 310 MPa
@Thickness 4.99 - 6.00 mm
Temper T651; Standard EN 485-2
 350 MPa
@Thickness 4.99 - 20.0 mm
Typical Strength
 350 MPa
@Thickness 20.0 - 80.0 mm
Typical Strength
Tensile Strength, Yield >= 240 MPa
@Strain 0.2 %,
Thickness 12.5 - 60.0 mm
Temper T651; Standard EN 485-2
 >= 240 MPa
@Strain 0.2 %,
Thickness 60.0 - 80.0 mm
Temper T651; Standard EN 485-2
 >= 255 MPa
@Strain 0.2 %,
Thickness 6.00 - 12.0 mm
Temper T651; Standard EN 485-2
 >= 260 MPa
@Strain 0.2 %,
Thickness 4.99 - 6.00 mm
Temper T651; Standard EN 485-2
 305 MPa
@Strain 0.2 %,
Thickness 4.99 - 20.0 mm
Typical Strength
 310 MPa
@Strain 0.2 %,
Thickness 20.0 - 80.0 mm
Typical Strength
Elongation at Break >= 7.0 %
@Thickness 60.0 - 80.0 mm
Temper T651; Standard EN 485-2
 >= 8.0 %
@Thickness 12.5 - 60.0 mm
Temper T651; Standard EN 485-2
 >= 9.0 %
@Thickness 6.00 - 12.0 mm
Temper T651; Standard EN 485-2
 >= 10 %
@Thickness 4.99 - 6.00 mm
Temper T651; Standard EN 485-2
 11 %
@Thickness 4.99 - 20.0 mm
Typical Elongation
 11 %
@Thickness 20.0 - 80.0 mm
Typical Elongation
Modulus of Elasticity 69.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000360 - 0.00000420 ohm-cmtemper T651
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 150 - 170 W/m-Ktemper T651
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 95.3 - 98.3 %as balance
Chromium, Cr <= 0.25 %
Copper, Cu <= 0.10 %
Iron, Fe <= 0.50 %
Magnesium, Mg 0.60 - 1.2 %
Manganese, Mn 0.40 - 1.0 %
Silicon, Si 0.70 - 1.3 %
Titanium, Ti <= 0.15 %
Zinc, Zn <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6082-T6
Aluminum 6061-T6; 6061-T651
Parkway Products Thixomolded® AM60A Magnesium
ALIMEX PLANAL 6082 T651 Aluminum Alloy
Aluminum 6082-T4

NCONS024 / 160287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.