MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.

Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good stiffness, high surface gloss, good formability. KR05NW is the no wax form of KR05 to facilitate printing and decorating.

Applications: Major applications include bottles, profiles, displays, containers, and unblended sheet.

Processing Recommendations:
Sheet Extrusion: Melt Temperature, 218°C maximum. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin. Blow Molding: 188-196°C for maximum melt strength. Generally no need to dry resin. Injection Blow Molding: Melt Temperature, 232°C maximum. Generally no need to dry resin.

Specification Data: FDA Regulation 21 CFR 177.1640. Suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50. UL 94HB.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Water Absorption 0.090 %0.090 %ASTM D570
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
7.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 26.0 MPa3770 psiType 1 @ 2 in/min; ASTM D638
Elongation at Break 160 %160 %Type 1 @ 2 in/min; ASTM D638
Flexural Yield Strength 34.0 MPa4930 psiASTM D790
Flexural Modulus 1.413 GPa204.9 ksiASTM D790
Izod Impact, Notched 0.410 J/cm
@Thickness 3.17 mm
0.768 ft-lb/in
@Thickness 0.125 in
ASTM D256
Impact Test 29.7 J
@Thickness 3.17 mm
21.9 ft-lb
@Thickness 0.125 in
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C163 °FASTM D648
Vicat Softening Point 87.0 °C189 °FCondition B (50N); ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 218 °C<= 424 °Fsheet extrusion
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USP Class VI YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® KR03BR SBC

PCHEVK65 / 20286

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.