MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low to high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.016 cm/cm0.015 - 0.016 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.012 - 0.013 cm/cm0.012 - 0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 54.1 MPa7850 psiASTM D638
Elongation at Break 39 %39 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 85.8 MPa12400 psiASTM D790
Flexural Modulus 2.74 GPa397 ksiASTM D790
Izod Impact, Notched 0.520 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.974 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+12 ohm-cm<= 1.00e+12 ohm-cmASTM D257
Surface Resistance <= 1.00e+12 ohm<= 1.00e+12 ohmASTM D257
Static Decay 0.40 sec0.40 sec(Mil-B-81705C), 12% RH, 5000kV to 50kV
Shielding Effectiveness  5.0 dB
@Frequency 1e+10 Hz
5.0 dB
@Frequency 1e+10 Hz
1/8 thickness
 10 dB
@Frequency 5.00e+9 Hz
10 dB
@Frequency 5.00e+9 Hz
1/8 thickness
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C>= 473 °FUnannealed; ASTM D648
 
Descriptive Properties
FeaturesElectromagnetic Shielding (EMI)
Filler / ReinforcementStainless Steel Fiber
FormsPellets
Generic MaterialNylon 6/12
Generic NamePolyamide 6/12 Copolymer (Nylon 6/12)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAerospace Applications
 Automotive Electronics
 Computer Components
 Connectors
 Electrical Housing
 Electrical/Electronic Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
Avient Bergamid™ AB700 UF Polyamide 66/6 Copolymer (Nylon 66/6)
LATI LATAMID 68 H2 G/30 30% Glass Fiber, Heat-Stabilized Nylon 66 Copolymer (Pac)
Teknor Apex Chemlon 275 Nylon 6, Copolymer Impact Modified
AdvanSix Aegis® HCA95YP Nylon 6/6,6 Extrusion Grade Copolymer

PH0POL1344 / 145913

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.