Varcum 29738 is a two-step, powder phenolic resin. APPLICATION: Molded brake block formulations. FEATURES: - Provides high heat resistance with excellent durability and wear resistance.
- Fast cure and short flow characteristics permit fast press cycles and high rates of brake block production.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |