MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
CHT Group QSil 563 Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 563 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairable.

Key Features:

  • 100% solids
  • Excellent thermal conductivity

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.07 g/ccUncatalyzed, QSil 563A
 2.13 g/ccUncatalyzed, QSil 563B
Viscosity 4000 cPUncatalyzed, QSil 563A
 5200 cPUncatalyzed, QSil 563B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 46Cure 15 minutes at 150°C
Tensile Strength 120 psiCure 15 minutes at 150°C
Elongation at Break 55 %Cure 15 minutes at 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.52e+15 ohm-cm
Dielectric Constant 4.57
@Frequency 1000 Hz
Dielectric Strength 18.1 kV/mm
Dissipation Factor 0.0070
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.880 W/m-K
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
Flammability, UL94 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 150 °C
As Tested
Gel Time 140 minCatalyzed
 
Descriptive Properties
ColorWhiteUncatalyzed, QSil 563A
 YellowUncatalyzed, QSil 563B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PACC2101 / 199489

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.