MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultramid® STAR SX 216 V50 NATURAL Nylon 6, 50% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Ultramid® STAR SX 216 V50 NATURAL is based on a patented high flow polyamide 6 resin, reinforced with 50% of glass fiber, for injection molding. Due to its outstanding flow characteristics, this grade allows more freedom in mold and part design versus a standard polyamide solutions.

Availability: Africa & Middle East; Asia Pacific; North America

Filler/Reinforcement: Glass Fiber, 50% Filler by Weight

Features: Good Dimensional Stability; Heat Stabilized – Inorganic; High Flow; High Stiffness; Outstanding Surface Finish

Uses: Consumer Applications; Electrical/Electronic Applications; Industrial Applications; Sporting Goods

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6-GF50

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183
Water Absorption 0.75 %
@Time 86400 sec
0.75 %
@Time 24.0 hour
ISO 62
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0015 cm/cm0.0015 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 230 MPa33400 psiISO 527-2
Elongation at Break 2.6 %2.6 %ISO 527-2
Tensile Modulus 17.0 GPa2470 ksiISO 527-1
Flexural Modulus 15.5 GPa2250 ksiISO 178
Izod Impact, Notched (ISO) 14.9 kJ/m²7.10 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 90.3 kJ/m²43.0 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 8.40 J/cm²40.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.49 J/cm²7.10 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 500 V500 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FUnannealed; ISO 75-2/A
Flammability, UL94  HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
IEC 60695-11-10,-20
 HB
@Thickness 3.30 mm
HB
@Thickness 0.130 in
IEC 60695-11-10,-20
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 235 °C446 - 455 °F
Middle Barrel Temperature 235 - 245 °C455 - 473 °F
Front Barrel Temperature 245 - 250 °C473 - 482 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2040 / 310733

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.