MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCO® 642 Aluminum-Silicon-Copper Alloy, Extruded-Drawn-Stress Relieved (HR-50), 1/2" to 1"
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: A wrought aluminum-silicon-copper alloy, Ampco 642 alloy has excellent capacity for hot forming, with a hot forgeability rating of 80 and a machinability rating of 60. Joining, using the brazing and arc welding methods, is only fair. Soldering and oxyacetylene welding are not recommended.

Applications: valve seats and stems; marine hardware; pole line hardware; bushings and bearings; cams; bolts and nuts; valve bodies and similar components

Key Words: ASTM B-150 C64200; Federal QQ-C-465 CA642; Military A-15939A Comp.1; AMS 4634 (thru 3")
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.69 g/cc
Density 7.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 86
Tensile Strength, Ultimate 586 MPa
Tensile Strength, Yield 310 MPa
Elongation at Break 12 %
Modulus of Elasticity 110 GPa
Modulus of Rigidity 41.0 GPa
Poissons Ratio 0.34Calculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000188 ohm-cm
@Temperature 20.0 °C
8% I.A.C.S.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 45.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 7.0 %
Copper, Cu 91 %
Silicon, Si 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK 275 Cast UNS C95900 Aluminum Bronze
MetalTek C86300 High Tensile Manganese Bronze
Aluminum Silicon Bronze, UNS C64200
Ampco Metal AMPCO® 642 Aluminum-Silicon-Copper Alloy, Hot Extruded (M-30), 3" to 4"
Oxygen-free Copper (OF), UNS C10200, OS050 temper, flat products, rod, tubing, and shapes

NAMPCO30 / 14984

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.