MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Marco Polo MARPOL LL6S 801 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: MARPOL® LL6S 801 is a linear low density polyethylene film resin. Films made from this Super Strength hexene copolymer exhibit excellent tear and impact strength.

Recommended Applications: Blown film extrusion and blown stretch wrap film.

Additives: Antiblock – no, Slip – no.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D1505
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.96 MPa1300 psiASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa1400 psiASTM D882
Film Elongation at Break, MD 630 %630 %ASTM D882
Film Elongation at Break, TD 720 %720 %ASTM D882
1% Secant Modulus 165 MPa24000 psiMD; ASTM D882
 186 MPa27000 psiTD; ASTM D882
Elmendorf Tear Strength, MD 18.1 g/micron460 g/milASTM D1922
Elmendorf Tear Strength, TD 23.6 g/micron600 g/milASTM D1922
Dart Drop Test 330 g0.728 lbASTM D1709
Film Tensile Strength at Break, MD 62.7 MPa9100 psiASTM D882
Film Tensile Strength at Break, TD 51.0 MPa7400 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 17 %17 %ASTM D1003
Gloss 37 %37 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO139 / 283736

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.