MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® B-202 Fluoroelastomer (FKM)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Viton® B-202 is a low viscosity, B-type gum polymer that demonstrates improved processing and rheology when compared with existing fluoroelastomers. Viton® B-202 is designed to be cured with either Viton® Curative #30 or Viton® Curative #50. When using Viton® Curative #30, use Viton® Curative #20 in a ratio of about 1.8 Viton® Curative #30 to Viton® Curative #20. When using Viton® Curative #50, use 0.3–0.5 phr of Viton® Curative #20 to ensure a fast cure rate. Note that Viton® Curative #20 can be difficult to mix into low viscosity stocks, such as those based on Viton® B-202, and careful attention needs to be paid to mixing procedures. Compared with other B-family terpolymers, Viton® B-202 provides:
  • Low viscosity
  • Improved processing
  • Increased mold flow
  • Excellent mold release

Applications:

  • Transfer and injection molding of complex shapes
  • Extrusions (e.g., fuel hose and tubing)
  • Solution coatings of fabrics, tanks or chemical containers

Viton® B-202 can be blended with other Viton® types to modify viscosity, enhance processability and/or improve flow.

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.84 g/cc
Mooney Viscosity 20
@Temperature 121 °C
ML 1 + 10; ASTM D1646
 
Descriptive Properties
Chemical CompositionTerpolymer of hexafluoropropylene, vinylidene fluoride, and tetrafluoroethylene
ColorSilver-gray, translucent
OdorNone
Physical FormSlab
SolubilityLow molecular weight esters and ketones
Storage StabilityExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® A-HV Fluoroelastomer (FKM)
Chemours Viton® AL-300 Fluoroelastomer (FKM)
Chemours Viton® AL-600 Fluoroelastomer (FKM)
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 8575 FFKM Perfluoroelastomer

PDVDA21 / 33990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.