Physical Properties | Metric | English | Comments |
---|
Density | 1.58 g/cc | 0.0571 lb/in³ |
Water Absorption | 0.500 % @Time 86400 sec | 0.500 % @Time 24.0 hour |
Moisture Absorption at Equilibrium | 1.20 % | 1.20 % |
Linear Mold Shrinkage, Flow | 0.00300 cm/cm @Thickness 2.00 mm | 0.00300 in/in @Thickness 0.0787 in |
Linear Mold Shrinkage, Transverse | 0.00800 cm/cm @Thickness 2.00 mm | 0.00800 in/in @Thickness 0.0787 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 173 MPa | 25100 psi |
| 240 MPa | 34800 psi |
Elongation at Break | 2.60 % | 2.60 % |
| 3.70 % | 3.70 % |
Tensile Modulus | 13.2 GPa | 1910 ksi |
| 17.1 GPa | 2480 ksi |
Flexural Strength | 270 MPa | 39200 psi |
| 350 MPa | 50800 psi |
Flexural Modulus | 11.2 GPa | 1620 ksi |
| 16.0 GPa | 2320 ksi |
Poissons Ratio | 0.400 | 0.400 |
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C | 7.61 ft-lb/in² @Temperature -22.0 °F |
| 17.0 kJ/m² @Temperature 23.0 °C | 8.09 ft-lb/in² @Temperature 73.4 °F |
| 18.0 kJ/m² @Temperature -30.0 °C | 8.57 ft-lb/in² @Temperature -22.0 °F |
| 21.0 kJ/m² @Temperature 23.0 °C | 9.99 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact Unnotched | 9.10 J/cm² @Temperature -30.0 °C | 43.3 ft-lb/in² @Temperature -22.0 °F |
| 9.50 J/cm² @Temperature -30.0 °C | 45.2 ft-lb/in² @Temperature -22.0 °F |
| 9.50 J/cm² @Temperature 23.0 °C | 45.2 ft-lb/in² @Temperature 73.4 °F |
| 11.0 J/cm² @Temperature 23.0 °C | 52.3 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C | 6.66 ft-lb/in² @Temperature -22.0 °F |
| 1.50 J/cm² @Temperature -30.0 °C | 7.14 ft-lb/in² @Temperature -22.0 °F |
| 1.50 J/cm² @Temperature 23.0 °C | 7.14 ft-lb/in² @Temperature 73.4 °F |
| 2.10 J/cm² @Temperature 23.0 °C | 9.99 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.00e+12 ohm-cm @Thickness 1.00 mm | 1.00e+12 ohm-cm @Thickness 0.0394 in |
Dielectric Strength | 20.0 kV/mm @Thickness 1.00 mm | 508 kV/in @Thickness 0.0394 in |
| 28.0 kV/mm @Thickness 1.00 mm | 711 kV/in @Thickness 0.0394 in |
Arc Resistance | 120 - 180 sec @Thickness 3.00 mm | 120 - 180 sec @Thickness 0.118 in |
Comparative Tracking Index | 400 - 599 V @Thickness 3.00 mm | 400 - 599 V @Thickness 0.118 in |
Hot Wire Ignition, HWI | 7.00 - 15.0 sec @Thickness 0.750 mm | 7.00 - 15.0 sec @Thickness 0.0295 in |
| 7.00 - 15.0 sec @Thickness 3.00 mm | 7.00 - 15.0 sec @Thickness 0.118 in |
| 15.0 - 30.0 sec @Thickness 1.50 mm | 15.0 - 30.0 sec @Thickness 0.0591 in |
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm | >= 120 arcs @Thickness 0.0295 in |
| >= 120 arcs @Thickness 1.50 mm | >= 120 arcs @Thickness 0.0591 in |
| >= 120 arcs @Thickness 3.00 mm | >= 120 arcs @Thickness 0.118 in |
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min @Thickness 3.00 mm | 0.394 - 1.00 in/min @Thickness 0.118 in |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature 23.0 - 55.0 °C | 6.67 µin/in-°F @Temperature 73.4 - 131 °F |
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C | 55.6 µin/in-°F @Temperature 73.4 - 131 °F |
Melting Point | 260 °C | 500 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F |
UL RTI, Electrical | 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 140 °C @Thickness 1.50 mm | 284 °F @Thickness 0.0591 in |
| 140 °C @Thickness 3.00 mm | 284 °F @Thickness 0.118 in |
UL RTI, Mechanical with Impact | 130 °C @Thickness 0.750 mm | 266 °F @Thickness 0.0295 in |
| 130 °C @Thickness 1.50 mm | 266 °F @Thickness 0.0591 in |
| 130 °C @Thickness 3.00 mm | 266 °F @Thickness 0.118 in |
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 140 °C @Thickness 1.50 mm | 284 °F @Thickness 0.0591 in |
| 140 °C @Thickness 3.00 mm | 284 °F @Thickness 0.118 in |
Flammability, UL94 | HB @Thickness 0.750 mm | HB @Thickness 0.0295 in |
| HB @Thickness 1.50 mm | HB @Thickness 0.0591 in |
| HB @Thickness 3.00 mm | HB @Thickness 0.118 in |
Flame Spread | 0.000 mm/min @Thickness 2.00 mm | 0.000 in/min @Thickness 0.0787 in |
Glow Wire Ignition Temperature | 700 °C @Thickness 0.750 mm | 1290 °F @Thickness 0.0295 in |
| 700 °C @Thickness 1.50 mm | 1290 °F @Thickness 0.0591 in |
| 750 °C @Thickness 3.00 mm | 1380 °F @Thickness 0.118 in |
Glow Wire Flammability Index | 675 °C @Thickness 0.750 mm | 1250 °F @Thickness 0.0295 in |
| 675 °C @Thickness 1.50 mm | 1250 °F @Thickness 0.0591 in |
| 960 °C @Thickness 3.00 mm | 1760 °F @Thickness 0.118 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F |
Melt Temperature | 285 - 305 °C | 545 - 581 °F |
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 4.00 hour | 4.00 hour |
|
Descriptive Properties |
---|
Additive | Heat Stabilizer |
| Lubricant |
Agency Ratings | ASTM, D6779 PA012G50 |
| RoHS Compliant |
| SAE, J1639 PA1116 |
Appearance | Black |
Automotive Material Specification | GM GMW3038P-PA66-GF50H |
| GM GMW3038P-PA66-GF50J |
| Li Auto QLiA53100058 |
| Renault AS25a |
| Stellantis MS-DB-41 CPN 4967 |
| Tesla TM-1006 v3 - 201150 |
| Toyota TSM5603G, Class 2C, Rev 5 (compliance) |
Features | Fatigue Resistant |
| Good Mold Release |
| Heat Stabilized |
| High Flow |
| High Rigidity |
| High Strength |
| Hydrolysis Resistant |
| Lubricated |
Forms | Pellets |
Processing Method | Injection Molding |
Region | North America, Europe, Asia Pacific |
UL File Number | E70062 |