MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Soluble Oil HD
Categories: Fluid; Lubricant

Material Notes: Soluble Oil HD is a chlorinated, heavy-duty metalworking fluid designed to emulsify easily and form a stable emulsion when mixed with water. It provides excellent cooling and lubricity for medium- to heavy-duty cutting and grinding of ferrous and non-ferrous metals, resulting in extended tool life and good surface finishes on the machined parts. Soluble Oil HD is formulated with naphthenic base oils and fortified with emulsifiers that form a stable emulsion when mixed with soft, medium or hard water. The high specific heat of water and the excellent metal-wetting ability of the emulsion provide excellent cooling and lubricity for most machining operations. This promotes longer tool life by reducing friction between the cutting tool and the workpiece and by dissipating heat. Antiwear and antiweld additives provide extra protection for heavy-duty machining operations. Soluble Oil HD provides excellent antiwear properties and good rust protection for both the cutting tool and the parts being machined. It contains a biocide to combat a wide spectrum of microorganisms, resulting in longer sump life and good odor control. It has very low foaming tendency, which is an advantage in high-speed machining and grinding operations.

Applications: Soluble Oil HD is recommended for medium- to heavy-duty machining operations with water hardness up to 300 ppm. Typical applications include:

  • Broaching
  • Milling
  • Deep hole drilling (gun drilling)
  • Reaming
  • Gear hobbing and gear shaping
  • Sawing
  • Grinding
  • Tapping
Features/Benefits:
  • Excellent cooling and lubricating properties
  • Excellent antiwear and antiweld properties
  • Helps extend cutting tool life
  • Good surface finish
  • Emulsifies easily with water
  • Forms a stable emulsion
  • Good rust protection
  • Good antifoam properties

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.958 g/cc
Density 7.98 lb/gal
pH 9.65% (1:20) dilution
Viscosity Measurement 79Index
Saybolt Viscosity at 100°F 225 SUS
Saybolt Viscosity at 210°F 46.7 SUS
Kinematic Viscosity at 40°C (104°F) 43.5 cSt
Kinematic Viscosity at 100°C (212°F) 6.1 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -20.0 °C
Flash Point 177 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 2.2 %
 
Descriptive Properties
ColorBlue-Green
Composition3.3%Fatty Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5268 / 198521

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.