MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Clariant 6008 L Nylon 6, High Impact, Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65
Tensile Strength, Yield 5800 psiASTM D638
Elongation at Yield 350 %ASTM D638
Flexural Modulus 150000 psiASTM D790
Izod Impact, Notched 17.0 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 410 - 413 °F
Deflection Temperature at 0.46 MPa (66 psi) 208 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 480 - 510 °F
Middle Barrel Temperature 480 - 510 °F
Front Barrel Temperature 490 - 520 °F
Nozzle Temperature 490 - 525 °F
Melt Temperature 490 - 520 °F
Mold Temperature 125 - 175 °F
Dry Time 2 - 4 hour
@Temperature 79.4 °C
to ensure moisture content is less than 0.2%
Injection Pressure 600 - 900 psiSecondary
 1000 - 1500 psiInitial
Back Pressure 50.0 - 250 psi
Shot Size 30 - 80 %
Screw Speed 20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Akro-Plastic Akromid® B3 3 S3 10 black 950063 PA 6 Dry
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM

PCLAR019 / 82144

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.