The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC5056 is a polypropylene random copolymer, with high gloss, excellent clarity, balance of rigidity and impact. Typical customer applications are injection molding of high clarity containers, house wares.Information provided by LyondellBasell. |