MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper-Cobalt-Beryllium alloy, UNS C17500, HTR (Proprietary mill hardening) Temper
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability.

Applications: fuse clips, fasteners, springs, switch and relay parts, electrical conductors, welding equipment.

HTR temper strip.

Key Words: BeCu; low beryllium copper, C112, ISO CuCo2Be, CEN CW104C, A3/1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 98 - 103
Tensile Strength, Ultimate 825 - 1035 MPa
Tensile Strength, Yield 760 - 965 MPa
@Strain 0.2 %
Elongation at Break 1.0 - 4.0 %In 50 mm
Modulus of Elasticity 125 - 130 GPa
Fatigue Strength 240 - 260 MPa
Machinability 40 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000029 - 0.0000038 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 120 BTU-in/hr-ft²-°F
Melting Point 1030 - 1070 °C
Solidus 1030 °C
Liquidus 1070 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 980 °CHot-Shortness Temperature
Solution Temperature 900 - 925 °CLarge sections, 1 hour per inch or fraction of an inch
 900 - 955 °C10 minutes, water quench
Aging Temperature 425 °C3-6 hours, for maximum strength
 470 - 495 °CCommercial practice, 2-3 hours
Hot-Working Temperature 700 - 925 °C
Precipitation Temperature >= 900 °F
@Time 7200 sec
Air
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.40 - 0.70 %
Cobalt, Co 2.4 - 2.7 %
Copper, Cu 96.9 %
Iron, Fe >= 0.10 %
Other, total >= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper-Cobalt-Beryllium alloy, UNS C17500, TB00 Temper strip, rod, bar, plate, tubing, forged products
Copper-Cobalt-Beryllium alloy, UNS C17500, TF00 Temper strip, rod, bar, plate, tubing, forged products
Copper-Cobalt-Beryllium alloy, UNS C17500, H04 Temper rod, bar, plate, tubing
Copper-Cobalt-Beryllium alloy, UNS C17500, TH04 Temper strip, rod, bar, plate, tubing
Copper-Cobalt-Beryllium alloy, UNS C17500, H04 Temper strip

MC17500b6 / 10899

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.