MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exterex™ A34 Synthetic Fluid
Categories: Fluid; Lubricant

Material Notes: Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low volatilities. Esterex™ Adipate Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many automotive and industrial lubricant applications. These esters are ideal in high-temperature conditions, such as reciprocating air compressors, where discharge valve cleanliness is required.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc
@Temperature 15.6 °C
0.0333 lb/in³
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 137137Index; ASTM D2270
Kinematic Viscosity 1970 cSt
@Temperature -40.0 °C
1970 cSt
@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 12 cSt12 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.2 cSt3.2 cStASTM D445
Evaporation Loss 37 %
@Temperature 205 °C,
Time 23400 sec
37 %
@Temperature 401 °F,
Time 6.50 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.080<= 0.080[mg KOH/g]; ASTM D974 (mod)
 
Thermal PropertiesMetricEnglishComments
Pour Point -60.0 °C-76.0 °FASTM D5950/D97
Flash Point 170 °C338 °FPMCC; ASTM D92
 199 °C390 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.44871.4487ASTM D1218
 
Descriptive Properties
Aniline Point14.4°FASTM D611
Biodegradation (%)78.5OECD 301F
Color<0.5ASTM D1500
CompositionWater<1000 ppm, ASTM D6304 (mod)
Density Correction Factor0.000733 (g/cc)/°CASTM D1250
Elastomer Compatibility (%)-14.9Nitrile Tensile Strength Change, ASTM D471
 -16Nitrile Hardness Change, ASTM D471
 17.2Nitrile Volume Change, ASTM D471
 -2.4Fluoroelastomer Elongation Change, ASTM D471
 -22Fluoroelastomer Tensile Strength Change, ASTM D471
 -22.5Polyacrylate Elongation Change, ASTM D471
 -24Polyacrylate Hardness Change, ASTM D471
 -30.9Nitrile Elongation Change, ASTM D471
 42.1Polyacrylate Volume Change, ASTM D471
 -45Polyacrylate Tensile Strength Change, ASTM D471
 -7Fluoroelastomer Hardness Change, ASTM D471
 8.6Fluoroelastomer Volume Change, ASTM D471
Fire Point478°FCOC, ASTM D92
Hydrolytic Stability, TAN Change0.11 mg KOH/gASTM D2619
Kauri-Butanol Value84.5ASTM D1133
Noack Volatility (%)20.4ASTM D5800/DIN 51581
RPVOT>1210 minWith AO, ASTM D2272

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gabriel Fluorolube® GR-290 CTFE Fluoropolymer Grease
Dow MOLYKOTE® 1292 LONG LIFE BEARING GREASE
Nye Lubricants UniFlor 8310 (472) (UF) Synthetic Oil
Lubriplate 68-P Semi-Synthetic Refrigeration Compressor Oil
Gabriel Versamid® 280B75 Polyamide Resin

PEX99700 / 175936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.