MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim ZDEC (EZ)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C10 H20 N2 S4 -Zn

Properties : White or light yellow powders, soluble in 1%NaOH solution, carbon disulfide, bezene, chloroform, insoluble in gasoline.

Application : A fast curing accelerator for natural, synthetic rubber and latex, especially suitable for butyl rubber, EPDM rubber and latex. Non-toxic, inodorous, it can be used as white or color and transparent rubber manufactures.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 361.9 g/mol361.9 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 174 °C>= 345 °F
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn 17 - 19 %17 - 19 %
 
Descriptive Properties
AppearanceWhite or light yellow powders
Heating Loss<0.4%
Residue<0.1%150µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI076 / 317360

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.