MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper Alloy, UNS C18135, TX00 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Spinodal Hardened-Low Strength (ATLS)

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability –Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed

Common Fabrication Processes: Bending, Cold working, Drawing, Extruding, Forging, Forming, Heading, Hot working, Rolling, Upsetting

Typical Uses: Electrical Applications Where Resistance to Softening at High Temperatures is Required; Electronic Stud Bases; Fuse Clips; High Strength-High Conductivity Wire; Switch Gear; Casting Molds; Cold Headed Parts; Aerospace Conductors

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 9494
Tensile Strength 372 MPa54000 psi
Tensile Strength, Yield 248 MPa36000 psi0.5% Ext
Elongation at Break 28 %28 %
Tensile Modulus 138 GPa20000 ksi
Modulus of Rigidity 51.7 GPa7500 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000187 ohm-cm0.00000187 ohm-cm92% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 30.3 W/m-K210 BTU-in/hr-ft²-°F
Melting Point <= 1080 °C<= 1976 °F
Liquidus 1080 °C1976 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 927 - 960 °C
@Time 60.0 sec
1700 - 1760 °F
@Time 0.0167 hour
Water
Hot-Working Temperature 816 - 927 °C1500 - 1700 °F
Precipitation Temperature >= 510 °C>= 950 °FAir
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 0.20 - 0.60 %0.20 - 0.60 %
Chromium, Cr 0.20 - 0.60 %0.20 - 0.60 %
Copper, Cu 98.8 - 99.6 %98.8 - 99.6 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC18135x4 / 291629

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.