MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC NORYL™ Resin HMC1010 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL HMC1010 compound is based on Polyphenylene Ether (PPE) resin containing 10% carbon fiber. Added features of this grade include: Electrically Conductive, Non-Chlorinated, Non-Brominated Flame Retardant.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Non-Chlorinated,Non-Brominated,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm
@Thickness 3.20 mm
0.00050 - 0.0015 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0015 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0015 - 0.0030 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D785
Tensile Strength at Break 71.0 MPa10300 psi5 mm/min; ASTM D638
Tensile Strength, Yield 79.0 MPa11500 psi5 mm/min; ASTM D638
Elongation at Break 3.0 %3.0 %5 mm/min; ASTM D638
Flexural Strength 103 MPa14900 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 6.89 GPa999 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 69.0 J50.9 ft-lbASTM D256
Izod Impact, Unnotched 2.40 J/cm4.50 ft-lb/inASTM D4812
Taber Abrasion, mg/1000 Cycles 8383CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8000 ohm-cm8000 ohm-cmASTM D257
Surface Resistance 13000 ohm13000 ohmASTM D257
Static Decay <= 0.010 sec<= 0.010 sec5000V to <50V; FTMS101B
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
@Thickness 6.40 mm
232 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
@Thickness 6.40 mm
221 °F
@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94  V-1
@Thickness 2.00 mm
V-1
@Thickness 0.0787 in
UL 94
 5VA
@Thickness 2.00 mm
5VA
@Thickness 0.0787 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 280 °C491 - 536 °F
Zone 2 230 - 275 °C446 - 527 °F
Zone 3 245 - 280 °C473 - 536 °F
Melt Temperature 255 - 280 °C491 - 536 °FInjection Molding
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 90.0 - 95.0 °C194 - 203 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82332 / 290279

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.