MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro DESMODUR® MD15120-F + BAYTEC® D15-F + BAYTEC® XL B-F, 65A Polyurethane, MDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccBAYTEC® XL B-F
 1.15 g/cc1.15 g/ccDESMODUR® MD15120-F
 1.18 g/cc1.18 g/ccBAYTEC®D15-F
 1.20 g/cc1.20 g/cc
Viscosity 30 cP30 cPBAYTEC® XL B-F
 390 cP390 cPBAYTEC®D15-F
 700 cP700 cPDESMODUR® MD15120-F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565DIN 53505
 60
@Temperature 80.0 °C
60
@Temperature 176 °F
DIN 53505
 69
@Temperature -5.00 °C
69
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 35.0 MPa5080 psiDIN 53504
Tensile Stress at Strain 0.800 MPa
@Strain 10 %
116 psi
@Strain 10 %
DIN 53504
Elongation at Break 460 %460 %DIN 53504
100% Modulus 2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
DIN 53504
200% Modulus 3.00 MPa
@Strain 200 %
435 psi
@Strain 200 %
DIN 53504
300% Modulus 4.80 MPa
@Strain 300 %
696 psi
@Strain 300 %
DIN 53504
Resilience 5555[%]; DIN 53512
Tear Strength 23.0 kN/m131 pliwith nick; ISO 34-1
 42.1 kN/m240 pliwithout nick; ISO 34-1
Abrasion 3030[mm3]; ISO 4649
Compression Set 23 %
@Temperature 70.0 °C,
Time 79200 sec
23 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FBAYTEC® XL B-F
 80.0 °C176 °FDESMODUR® MD15120-F
 80.0 °C176 °FBAYTEC®D15-F
Mold Temperature 100 °C212 °F
Pot Life 7.50 min7.50 min
 
Descriptive Properties
AppearancesolidDESMODUR® MD15120-F
 solidBAYTEC®D15-F
 solidBAYTEC® XL B-F
Content10.5-10.9%NCO
 100Parts by weight of prepolymer
 2.7Parts by weight of BAYTEC®XL B-F
 95Parts by weight of BAYTEC®D15-F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0434 / 202217

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.