MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Hysol EA 9394/C-2 Paste Adhesive System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Elevated cure, thixotropic adhesive with structural properties to 450°F / 232°C.

Application: Structural Repair

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 165.5 MPa
Adhesive Bond Strength 24.0 MPa
@Temperature -55.0 °C
Tensile Lap Shear
 24.1 MPa
@Temperature 93.0 °C
Tensile Lap Shear
 34.5 MPa
@Temperature 25.0 °C
Tensile Lap Shear
Peel Strength 1.80 kN/mBell Peel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 232 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 93.0 °C
Pot Life 480 min
 
Descriptive Properties
ConsistencyModerate Viscosity
Form2 parts
Mix Ratio, Part A:Part B100:20
Peel StrengthLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 9394 Paste Adhesive System
Henkel Hysol EA 9395 Paste Adhesive System
Henkel Hysol EA 9825 Paste Adhesive System
Henkel Hysol EA 9396.6MD Paste Adhesive System
Henkel Hysol EA 9396/C-2 Paste Adhesive System

PHENK819 / 146824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.