MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Polykemi AB POLYblend 65FS PC/ABS-Blend
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:

Information provided by Polykemi AB

Key Words: PC/ABS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmISO 2577
Melt Index of Compound 25 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Elongation at Yield 5.0 %ISO/R527
Flexural Strength <= 95.0 MPaISO 178
Flexural Modulus 2300 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact, Notched 25.0 kJ/m²
@Temperature -20.0 °C
ISO 179
 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 105 °C120°C/h; ISO 75/1
Vicat Softening Point 115 °C
@Load 5.001 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
Glow Wire Test 650 °C
@Thickness 2.00 mm
IEC 695-2-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 100 - 110 °C
Dry Time 2 - 8 hourin circulation dryer
 2 - 8 hourin fresh-air dryer
 2 - 8 hourin desiccant air dryer
Injection Pressure 90.0 - 150 MPa
Back Pressure 0.500 - 1.50 MPa
 
Descriptive Properties
Holding Pressure20-50% of injection pressure
Injection SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polykemi AB POLYblend 65FS LB PC/ABS-Blend
Polykemi AB POLYblend 65FS GF20 PC/ABS-Blend
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Overview of materials for Polycarbonate, 20% Glass Filled

PPOLYK034 / 122759

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.