MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nickel Aluminum Bronze, UNS C63200, O50 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Hot Extruded

Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding; Good Suitability – Coated Metal Arc Welding, Spot Weld, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Soldering. Brazing, Seam Weld, Capacity for Being Cold Worked

Common Fabrication Processes: Hot Forming; Welding

Typical uses: Bolting; Fasteners, Sea Water; Nuts; Bearing Cages; Bushings; Cams; Sea Water Pump Bodies; Sea Water Valves; Shafts; Sleeve Bearings; Valve Stems; Drive Shafts, Marine Service

Applicable Specifications: Bar - ASTM B124/B124M; Electrode – Welding MILITARY MIL-E-23765/3, Welding AWS A5.6; Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Plate & Sheet - for Pressure Vessels, Condensers & Heat Exchangers ASTM B171/B171M, for Pressure Vessels, Condensers & Heat Exchangers ASME SB171; Rod – ASTM B124/B124M; Rod, Bar & Shapes - Aluminum Bronze ASTM B150/B150M, Aluminum Bronze ASME SB150; Shapes – ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.64 g/cc0.276 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  93
@Thickness 76.2 mm
93
@Thickness 3.00 in
 94
@Thickness 50.8 mm
94
@Thickness 2.00 in
 96
@Thickness 25.4 mm
96
@Thickness 1.00 in
Tensile Strength  703 MPa
@Thickness 76.2 mm
102000 psi
@Thickness 3.00 in
 710 MPa
@Thickness 50.8 mm
103000 psi
@Thickness 2.00 in
 724 MPa
@Thickness 25.4 mm
105000 psi
@Thickness 1.00 in
Tensile Strength, Yield  352 MPa
@Thickness 76.2 mm
51000 psi
@Thickness 3.00 in
0.5% Ext
 359 MPa
@Thickness 50.8 mm
52000 psi
@Thickness 2.00 in
0.5% Ext
 365 MPa
@Thickness 25.4 mm
53000 psi
@Thickness 1.00 in
0.5% Ext
Elongation at Break  22 %
@Thickness 25.4 mm
22 %
@Thickness 1.00 in
 24 %
@Thickness 50.8 mm
24 %
@Thickness 2.00 in
 24 %
@Thickness 76.2 mm
24 %
@Thickness 3.00 in
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 30 %30 %
Forgeability 70 %70 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000250 ohm-cm0.0000250 ohm-cm7% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.439 J/g-°C0.105 BTU/lb-°F
Thermal Conductivity 2.88 W/m-K20.0 BTU-in/hr-ft²-°F
Melting Point 1041 - 1060 °C1905 - 1940 °F
Solidus 1041 °C1905 °F
Liquidus 1060 °C1940 °F
Annealing Point 621 - 704 °C1150 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 816 - 899 °C1500 - 1650 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.7 - 9.5 %8.7 - 9.5 %
Copper, Cu 79.3 - 82.6 %79.3 - 82.6 %As Balance
Iron, Fe 3.5 - 4.3 %3.5 - 4.3 %
Lead, Pb <= 0.020 %<= 0.020 %
Manganese, Mn 1.2 - 2.0 %1.2 - 2.0 %
Nickel, Ni 4.0 - 4.8 %4.0 - 4.8 %
Silicon, Si <= 0.10 %<= 0.10 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC63200x3 / 293047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.