The viscosity of HumiSeal® coatings may be adjusted for application purposes, using a compatible thinner. HumiSeal® Thinners are blends of solvents, formulated to maintain the original system balance when added to the correct coating type. This HumiSeal® Thinners is in full compliance with the RoHS Directive 2002/95/EC.Information provided by Chase Electronic Coatings. |