MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton ARC 855 Abrasion Control Coating
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by brush or roller. ARC 855 may be applied at a minimum thickness of 250 microns (10 mills) per coat. Non-shrinking. 100% Solids. ARC 855 may be used alone, or in conjunction with other ARC composites. This two-coat system provides extended wear and predictable preventative maintenance. The cured ceramic composite provides outstanding chemical and abrasion resistance with a high gloss finish.

Benefits:

  • High gloss surface reduces dray, improves flow and pump efficiency
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion insures reliable performance with no undercutting or under film corrosion
  • Labor and downtime costs are reduced due to ease of application
  • No heat curing required
  • Performs well under fluctuating chemical environments

Suggested Uses:

  • Fans & Housings
  • Heat Exchangers
  • Hoppers
  • Hydropulpers
  • Pump Casings
  • Sand Filter Vessels
  • Structural Steel
  • Tanks and Vessels
  • Volutes
  • Wet Scrubbers
  • Valves
  • Coal Hoppers and Feeders
  • Waterboxes
  • Cooling Water Pumps
  • Wear Plates
  • Coal Screens
  • Impellers
  • Condensers
  • Vacuum Pumps
  • Pitted Tanks and Pipes
  • Pulp Dewatering Screws

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Hardness, Shore D 8585ASTM D2240
Tensile Strength at Break 23.4 MPa3400 psiASTM D638
Flexural Strength 55.2 MPa8000 psiASTM D790
Compressive Strength 82.7 MPa12000 psiASTM D695
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C26.0 µin/in-°FASTM C531
Maximum Service Temperature, Air 65.0 °C149 °FWet Service
 120 °C248 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  360 min
@Temperature 32.0 °C
6.00 hour
@Temperature 89.6 °F
Light Load
 600 min
@Temperature 32.0 °C
10.0 hour
@Temperature 89.6 °F
Overend Coat
 720 min
@Temperature 25.0 °C
12.0 hour
@Temperature 77.0 °F
Light Load
 720 min
@Temperature 32.0 °C
12.0 hour
@Temperature 89.6 °F
Full Load
 1200 min
@Temperature 25.0 °C
20.0 hour
@Temperature 77.0 °F
Overend Coat
 1440 min
@Temperature 16.0 °C
24.0 hour
@Temperature 60.8 °F
Light Load
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Full Load
 1440 min
@Temperature 32.0 °C
24.0 hour
@Temperature 89.6 °F
Full Chemical
 1920 min
@Temperature 16.0 °C
32.0 hour
@Temperature 60.8 °F
Overend Coat
 2160 min
@Temperature 10.0 °C
36.0 hour
@Temperature 50.0 °F
Light Load
 2520 min
@Temperature 10.0 °C
42.0 hour
@Temperature 50.0 °F
Overend Coat
 2880 min
@Temperature 16.0 °C
48.0 hour
@Temperature 60.8 °F
Full Load
 2880 min
@Temperature 25.0 °C
48.0 hour
@Temperature 77.0 °F
Full Chemical
 5760 min
@Temperature 10.0 °C
96.0 hour
@Temperature 50.0 °F
Full Load
 5760 min
@Temperature 16.0 °C
96.0 hour
@Temperature 60.8 °F
Full Chemical
 7680 min
@Temperature 10.0 °C
128 hour
@Temperature 50.0 °F
Full Chemical
Tack-Free Time  120 min
@Temperature 32.0 °C
2.00 hour
@Temperature 89.6 °F
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
 480 min
@Temperature 16.0 °C
8.00 hour
@Temperature 60.8 °F
 960 min
@Temperature 10.0 °C
16.0 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorBlack
 Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301/GF/30/TF/15 PPS, linear with glass fiber and PTFE
Chesterton ARC 982 100% Novolac acid resistant coating
BASF Procom® GC20H 250 Polypropylene
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend
3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild

PPTCHS039 / 138151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.