MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lubriplate 1200-2 Lithium Type Multi-Purpose Grease
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: This is a heavy-duty general purpose lithium type grease for both industrial and automotive applications. It provides a high film strength, shear stability, and AW & EP additives.

Applications: General-purpose grease.

1200-2 is available in Cartridges, Cans, Pails, 1/4 Drums & Drums.

Information provided by Lubriplate

Key Words: Part Number L0102-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 950 SUS
Kinematic Viscosity at 40°C (104°F) 183 cSt
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 265Unknown Amount of Work
Penetration P(60), 1/10 mm 295Unknown Amount of Work
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -25.0 °FApprox. Cold test
Dropping Point 400 °FASTM Test
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW/EP
NLGI Grade2
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ELM® White Lithium Biodegradable Lubricating Grease

WLUBR048 / 76094

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.