MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.

NOVA Chemicals' polyethylene resins are biologically and chemically inert.

Features: Good stiffness, Easy processability, Very good toughness and strength, Excellent seal properties, Low gel

Additives: Process stabilizer, Antiblock at 3400 ppm, Polymer process aid

Applications: Heavy duty shipping sacks requiring very good toughness and high stiffness, Industrial packaging, Industrial liners, Lamination film

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccASTM D 792
Thickness 25.0 micronsAs tested for properties on this data sheet
 25.0 - 150 micronsRecommended range for processing
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 9.00 MPaASTM D 882
Film Tensile Strength at Yield, TD 10.0 MPaASTM D 882
Film Elongation at Break, MD 520 %ASTM D 882
Film Elongation at Break, TD 700 %ASTM D 882
Elmendorf Tear Strength MD 290 gASTM D 1922
Elmendorf Tear Strength TD 490 gASTM D 1922
Elmendorf Tear Strength, MD 11.6 g/micronASTM D 1922
Elmendorf Tear Strength, TD 19.6 g/micronASTM D 1922
Dart Drop 20.5 g/micronASTM D 1709/A
Dart Drop Test 512 gF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 50.0 MPaASTM D 882
Film Tensile Strength at Break, TD 42.0 MPaASTM D 882
1% Secant Modulus, MD 174 MPaASTM D 882
1% Secant Modulus, TD 188 MPaASTM D 882
 
Optical PropertiesOriginal ValueComments
Haze 21 %ASTM D 1003
Gloss 33 %At 45°; ASTM D 2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 230 °CRecommended
Die Opening 0.0350 - 0.0800 inRecommended range
 
Descriptive Properties
Low Friction Puncture53 (J/mm)NOVA Chemicals test method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin

PNOV771 / 108896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.