MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt POLYCOR® 54X Series Gel Coat
Categories: Polymer; Thermoset

Material Notes: The 54X series gelcoat are formulated with a particular mix of polyester resins, for use in applications where sun exposure and weather conditions are a factor. They are suitable for boats, truck cabs, water slides and environments with humidity and direct sun exposure. This unique formulation is easier and quicker gloss recovery with less buffing time to achieve gloss.

Characteristics:

  • Very good resistance to yellowing and fading due to sun exposure
  • Resist to thermal change and weathering
  • May be used in submerged application
  • Chalking resistant
  • Easy to sand and polish

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 3300 - 5300 cPcolored, RVF #4 @ 20 rpm
 3500 - 5500 cPwhite and off white, RVF #4 @ 20 rpm
 
Processing PropertiesOriginal ValueComments
Cure Time 40.0 - 60.0 min
@Temperature 25.0 °C
Lay-up Time; tested @ 1,8% Norox MEKP 925 @ 25°C
Gel Time 10.0 - 18.0 min
@Temperature 25.0 °C
tested @ 1,8% Norox MEKP 925 à 25°C
 
Descriptive Properties
Sag ResistanceGood at 20 mils
Thixotropic Index>52/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9266 / 231861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.