MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical IP-40
Categories: Fluid

Material Notes: Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants or C5 products.

Uses: As a polyurethane foaming agent, it is increasingly used in place of Freon foaming agent.

CAS: 78-78-4 and 109-66-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.620 - 0.650 g/cc
@Temperature 15.6 °C
0.620 - 0.650 g/cc
@Temperature 60.1 °F
15.6/15.6°C; ASTM D287
Volatiles 100 %100 %n-Pentane
 100 %100 %Iso-Pentane
Vapor Pressure  0.568 bar
@Temperature 20.0 °C
426 torr
@Temperature 68.0 °F
Vapor Density=2.48, n-Pentane
 0.793 bar
@Temperature 20.0 °C
595 torr
@Temperature 68.0 °F
Vapor Density=2.48, Iso-Pentane
 
Thermal PropertiesMetricEnglishComments
Melting Point -160.5 °C-256.9 °FIso-Pentane
 -130.5 °C-202.9 °Fn-Pentane
Boiling Point 28.0 °C82.4 °FIso-Pentane
 36.0 °C96.8 °Fn-Pentane
Flash Point >= -49.0 °C>= -56.2 °F
Ignition Temperature 260 °C500 °FAutoignition
 
Descriptive Properties
ComponentsAROMATICS<20 ppm
 Aromatics<20 ppm
 Benzene<20 ppm
 BENZENE<20 ppm
 H2O<100 ppm
 H2O<100 ppm
 ISO-PENTANE37-43%
 iso-Pentane38-42%
 n-Pentane46-54%
 SULFUR<100 ppm
 Sulfur<1 ppm
 total olefin<400 ppm
 TOTAL OLEFINS<400 ppm
 total-Pentane>97%
 T-PENTANE>97%
Cu Corrosion1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ IP-40 High Density Polyethylene

PLAY771 / 148781

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.