NP515LS is a woven glass fabric combined with a high temperature phenolic resin. It is engineered to provide superior shrink characteristics at elevated temperatures, making it an ideal material for insulating gaskets. Having been tested and certified as a NEMA G-3 material, NP515LS also meets or exceeds the requirements of IEC 60893-3-4 PF GC 201.Information provided by Norplex-Micarta |
Glass Fiber, Phenolic, Micarta, NEMA G-3, IEC 60893-3-4 PF GC 201 |