MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech PP5220 Calcium Carbonate Filled Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Calcium Carbonate (CaCO3) Filler

Material Notes: Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Calcium Carbonate also offers advantages in appearance, gloss, and colorability due to its bright white color.

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
@Temperature 22.8 °C
ASTM D792
Filler Content 20 %
Linear Mold Shrinkage 0.015 in/in0.125inch wall
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4300 psiASTM D638
Elongation at Break 115 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus 220000 psisecant; ASTM D790
 285000 psitangent; ASTM D790
Izod Impact, Notched 0.700 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 12.0 ft-lb
@Temperature 22.8 °C
ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °FASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 75 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Amco PRIMATOP PP HOMO 350NA Injection Molding Polypropylene
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer
Spartech PP7220 Calcium Carbonate Filled High Impact Copolymer
Spartech PP5240 Calcium Carbonate Filled Homopolymer
Spartech EP6240 Filled and Reinforced Copolymer

PSPAR114 / 78736

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.