MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as sealability. It has very low gel content. It contains medium anitblocking, medium slip, processing aid, and LDPE additives. Its applications include: automatic packaging (FFS), liners, general purpose, and HDPE and LDPE blends.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM-D792
Melt Flow 0.68 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 930 %ASTM-D882
Film Elongation at Break, TD 1200 %ASTM-D882
Elmendorf Tear Strength MD 60 gASTM-D1922
Elmendorf Tear Strength TD 520 gASTM-D1922
Elmendorf Tear Strength, MD 1.58 g/micronASTM-D1922
Elmendorf Tear Strength, TD 13.68 g/micronASTM-D1922
Dart Drop 2.37 g/micronASTM-D1709
Dart Drop Test 90.0 gASTM-D1709
Film Tensile Strength at Break, MD 40.0 MPaASTM-D882
Film Tensile Strength at Break, TD 30.0 MPaASTM-D882
1% Secant Modulus, MD 160 MPaASTM-D882
1% Secant Modulus, TD 170 MPaASTM-D882
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM-D1003
Gloss 127 %Angle 60°; ASTM-D2457
 
Processing PropertiesOriginal ValueComments
Die Opening 0.180 - 0.250 cmBlown Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.0Blown Film Extrusion
 
Descriptive Properties
Mass Temperature (°C)190-210Blown Film Extrusion
Screen Package40/40100% pure
 40/60/40Blend
Temperature Profile (°C)180-210Blown Film Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
FKuR Kunststoff Terralene® HD 3505 Biobased Polyethylene
DuPont Selar® RB 215 Nylon Blend Barrier Resin
Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin
Chevron Phillips Marlex® 9656 HDPE Blown Film Resin

PBRAS855 / 106701

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.