MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Aktiplast® 8 Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Aktiplast 8 is a highly effective peptizing agent for the depolymerization of natural rubber

Use: In mastication the molecule chains of the rubber are split by a process in which atmospheric oxygen participates. This reduces their weight and decreases viscosity. Aktiplast 8 accelerates the mastication process, leading to important energy and time savings. In general, the effect increases with the temperature of the rubber. Aktiplast 8 is particularly suitable for NR and IR, on which it has a marked peptizing effect even at rubber temperatures of about 80 °C. It also peptizes synthetic rubber, such as SBR, IR and BR.

Application: Tires and technical goods, masticator for peptizing natural rubber at low and high temperatures

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
 
Thermal PropertiesMetricEnglishComments
Solidus 85.0 - 97.0 °C185 - 207 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Appearancebrown Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8247 / 208640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.