MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
ITW Chockfast® PHILLYBOND TA-30 Epoxy Tile Adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: PHILLYBOND TA-30 is a two component, high tack strength, epoxy adhesive specifically developed for the installation of vibration damping materials such as MLD-2 Tiles, RA, Saper, Isoper, PVC and other. Clamping or shoring is generally eliminated as TA-30 Adhesive will support in excess of 25 kg/sq.m. (5 lbs./sq.ft.) on overhead and vertical surfaces while curing takes place. TA-30 is excellent for grouting between damping tile sheets and for forming fillets at welds or seams. TA-30 is nontoxic and contains no solvents. Fumes and odors of mixed TA-30 are negligible thus facilitating usage in confined areas. Resistance to fresh water, salt water, crude and refined oils, gasoline, jet fuel, etc., is excellent. SURFACE PREPARATION: Surfaces must be clean and sound and free of oil, dirt, old paint and other foreign matter. Blast, abrade or clean surface for best adhesion. Final rinse of surfacewith Impax IXT 59 solvent helps to ensure complete removal of grease and oils.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 20ASTM D2583
Tensile Strength 3200 psiASTM D638
Compressive Strength 11000 psiASTM D695
Compressive Modulus 197000 psi
Adhesive Bond Strength 1274 psiLap shear vs. steel; ASTM D1002
 1700 psiPerpendicular to the bond; MIL-A-24456
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 22.0 °C
 360 hour
@Temperature 1.70 °C
Pot Life 90.0 min
@Temperature 22.2 °C
6 liters batch
Shelf Life 24.0 Month
 
Descriptive Properties
Colorblackhardener
 graymixed
 whiteresin
Mix Ratio by volume1 to 1Resin to hardener
Mix Ratio by weight100 to 88Resin to hardener
Resistance to High ImpactpassMIL-S-901
ViscosityThixotropic paste, trowelable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWC9037 / 239547

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.