MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Rogers Arlon Silicone Hose and Duct Material with Polyester Substrate (65390R042)  (discontinued **)
Categories: Polymer; Thermoset; Silicone

Material Notes: Side one - uncured silicone, 0.005 in., -0.001(0.1 mm, -0.01); Substrate - 6500 Polyester Fabric, 0.038 in. (0.97 mm) nominal; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.042 in +0.004,-0.001 (1.1 mm + 0.1,-0.03). Color: Red. Weight: 1695 g/m² ± 136 (50.0 oz./yd.² ± 4). Shelf Life: 6 months from date of manufacture at 21°C (70°F). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Peel strength is 62 kPa (9.0 psi).

Applications: Hose and duct material.

Information provided by the manufacturer, Arlon Silicone Technologies Division.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50 - 60
Tensile Strength, Ultimate 4.18 - 5.42 MPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 14.76 - 23.62 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 232 °C
Minimum Service Temperature, Air -56.6 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Silicone, Molded, Glass Fiber Filled
CHT Group QM 230 QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material

PASD63 / 24734

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.