MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Melos Mecoline I RDX 1223 F Radiation cross-linkable, halogen-free, flame retardant compound
Categories: Polymer; Thermoplastic

Material Notes: Radiation cross-linkable, halogen-free, flame retardant compound

Compound class: Insulation / sheathing

Compound category: RDX

Flame retardant: ATH

Standards: UL 3266, 3271; CSA AWM I A/B 1

Typical applications: This compound is an ideal choice for the insulation of heat-resistant wires and cables for applications in railway systems, nuclear power stations, engine compartments and other areas.

Features: Flame retardant; Halogen-free; Low smoke; High temperature resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccpressed plaques; DIN EN ISO 1183-1A
pH >= 4.8Corrosivity; IEC 60754-2
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 160 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 34pressed plaques; DIN ISO 7619-1
Tensile Strength >= 9.00 MPaextruded tapes; IEC 60811-501
 >= 14.0 MPacross-linked plaques or tapes, 100kGy; IEC 60811-501
 >= 9.45 MPa
@Temperature 158 °C,
Time 605000 sec
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
Elongation at Break 400 %cross-linked plaques or tapes, 100kGy; IEC 60811-501
 750 %extruded tapes; IEC 60811-501
 10 %
@Temperature 200 °C,
Time 900 sec
Hot set test, Residual, 0.2 Mpa; IEC 60811-507
 20 %
@Temperature 200 °C,
Time 900 sec
Hot set test, under load, 0.2 Mpa; IEC 60811-507
 727.5 %
@Temperature 158 °C,
Time 605000 sec
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.9
@Frequency 1000 Hz,
Temperature 20.0 °C
IEC 250
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -40.0 °C
Brittleness Temperature -21.0 °Ccross-linked plaques or tapes; ASTM D746-14
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 170 °CTool
 220 °CMaximum mass temperature
Zone 1 130 - 140 °C
Zone 2 150 - 160 °C
Zone 3 160 - 170 °C
Zone 4 160 - 170 °C
Zone 5 160 - 170 °C
Adapter Temperature 160 - 170 °C
Head Temperature 160 - 170 °C
Drying Temperature 60.0 - 70.0 °C
Dry Time 4.00 - 6.00 hour
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 30 %ASTM D 2863 A
 
Descriptive Properties
Cold bend testPassat -15°C, IEC 60811-504
Conductivity=2.0 µS/mmpressed plaques, IEC 60754-2
Main burning properties0Halogen content, IEC 754-1
Temperature index275°CASTM D 2863 D
Toxicity index1EN 50305

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS031 / 296138

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.