MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Entec Enflex® V1070A BLK UV TPV
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: Enflex V1070A BLK UV (thermoplastic vulcanizate) is a fully weatherable black EPDM/PP compound. It is designed to replace thermoset elastomers such as EPDM or polychloroprene, and traditional thermoplastic TPVs. Enflex V grades provide the performance of vulcanized rubber with the advantage of low-cost thermoplastic processing.

Availability: North America

Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Processability; Good Weather Resistance; High Heat Resistance; Low Compression Set; Oil Resistant; Ozone Resistant; Recyclable Material; Solvent Resistant; UV Resistant

Appearance: Black

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.972 g/cc0.0351 lb/in³ASTM D792
Maximum Moisture Content 0.0800.080
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  67
@Time 5.00 sec
67
@Time 0.00139 hour
Extruded; ASTM D2240
 70
@Time 5.00 sec
70
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 8.14 MPa1180 psiASTM D412
Tensile Stress 3.30 MPa
@Strain 100 %
479 psi
@Strain 100 %
ASTM D412
Elongation at Break 610 %610 %ASTM D412
Tear Strength 38.0 kN/m217 pliDie C; ASTM D624
Compression Set  32 %
@Temperature 70.0 °C,
Time 79200 sec
32 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 49 %
@Temperature 125 °C,
Time 252000 sec
49 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 158 °C317 °FASTM D1238
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 177 °C320 - 350 °FHopper, Extrusion
Rear Barrel Temperature 177 - 188 °C350 - 370 °F
Middle Barrel Temperature 182 - 193 °C360 - 380 °F
Front Barrel Temperature 188 - 199 °C370 - 390 °F
Nozzle Temperature 199 - 221 °C390 - 430 °F
Zone 1 171 - 191 °C340 - 375 °F
Zone 2 171 - 191 °C340 - 375 °F
Zone 3 171 - 191 °C340 - 375 °F
Zone 4 171 - 191 °C340 - 375 °F
Zone 5 171 - 191 °C340 - 375 °F
Adapter Temperature 191 - 210 °C375 - 410 °F
Die Temperature 191 - 210 °C375 - 410 °F
Melt Temperature 191 - 199 °C375 - 390 °FExtrusion
 199 - 232 °C390 - 450 °FInjection
Mold Temperature 10.0 - 48.9 °C50.0 - 120 °FInjection
Drying Temperature 82.2 °C180 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 5.17 - 8.96 MPa750 - 1300 psi
Cushion 0.508 - 1.27 cm0.200 - 0.500 in
Screw Speed 50 - 200 rpm50 - 200 rpmInjection
 100 - 200 rpm100 - 200 rpmExtrusion
 
Descriptive Properties
Dynamic Service Temperature266°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENTB661 / 311354

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.