MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bamberger Polymers Bapolene® 1030 Low Density Polyethylene Extrusion/Injection Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Description: This resin is a multipurpose extrusion/injection low density polyethylene with excellent processability and good stiffness. This product meets US FDA 21 CFR 177.1520.

Applications: Bottles; Caps; Closures; Profiles; Tubing.

Information provided by Bamberger Polymers.

Key Words: Food Contact Acceptable; Good Impact Resistance; Good Processability; Good Stiffness.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D-1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 410 %410 %ASTM D882
Film Elongation at Break, TD 500 %500 %ASTM D882
Secant Modulus, MD 0.169 GPa24.5 ksiASTM D882
Secant Modulus, TD 0.207 GPa30.0 ksiASTM D882
Elmendorf Tear Strength MD 360 g360 gASTM D-1922
Elmendorf Tear Strength TD 130 g130 gASTM D-1922
Dart Drop Test 90.0 g0.198 lbASTM D-1709
Film Tensile Strength at Break, MD 26.6 MPa3850 psiASTM D-882
Film Tensile Strength at Break, TD 18.3 MPa2650 psiASTM D-882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processExtrusion
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 108A Low Density Polyethylene Film Extrusion Resin
Bamberger Polymers Bapolene® 105F Low Density Polyethylene Film Resin
Bamberger Polymers Bapolene® 1052 Polyethylene, Injection Grade
Overview of materials for Low Density Polyethylene (LDPE), Molded
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene

PBP3B088 / 20800

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.