MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and the natural is laser transmissive.

- Black: A-6135 NL BK543
- Natural: A-6135 NL NT

Features: Good Chemical Resistance; Good Creep Resistance; Good Flow; Good Stiffness; High Stiffness; High Strength; Hot Water Moldability; Laser Weldable; Low Moisture Absorption

Uses: Automotive Applications; Automotive Electronics; Connectors; Electrical Parts; Housings

Availability: Africa & Middle East; Asia Pacific; Europe; North America; South America

Injection Rate: 3 to 6 in/sec
Holding Pressure: 50% of injection pressure

Information provide by Solvay Specialty Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183 Method A
Water Absorption 0.29 %0.29 %24 hrs; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 220 MPa31900 psiISO 527-2
Elongation at Break 2.5 %2.5 %ISO 527-2
Tensile Modulus 12.5 GPa1810 ksiISO 527-2
Flexural Strength 300 MPa43500 psi3.5%; ISO 178
Flexural Modulus 11.4 GPa1650 ksiISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 65.0 kJ/m²30.9 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 310 °C590 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 303 °C577 °FUnannealed; Flatwise; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 288 °C550 °FUnannealed; Flatwise; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 315 - 321 °C599 - 610 °F
Middle Barrel Temperature 315 - 321 °C599 - 610 °F
Front Barrel Temperature 327 - 332 °C621 - 630 °F
Melt Temperature 320 - 335 °C608 - 635 °F
Mold Temperature 65.0 - 93.0 °C149 - 199 °F
Drying Temperature 120 °C248 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %suggested max
 
Descriptive Properties
AppearanceBlack; Natural Color
FormsPellets
Processing MethodWater-Assisted Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)

PSOLVAY266 / 122564

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.