MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röhm CYROLITE® MD L40 Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: CYROLITE® MD L40 acrylic polymer is an amorphous thermoplastic molding compound based on polymethyl methacrylate (PMMA) for the medical diagnostic industry.

Typical properties of CYROLITE® MD acrylic polymers are:

  • Exceptional ultra-violet light transmittance
  • Superior optical clarity
  • Maximum flow characteristics
  • Excellent dimensional stability
  • Outstanding scratch resistance
  • Total cost-of-use advantage over glass
The special properties of CYROLITE® MD L40 are:
  • Highest melt flow rate
  • Medium levels of lubricant
Application: Used for injection molded thin-wall medical devices requiring UV spectroscopy for fluid evaluation.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Bulk Density 0.660 g/cc0.0238 lb/in³ASTM D1895
Water Absorption <= 0.30 %<= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 26 g/10 min
@Load 3.80 kg,
Temperature 230 °C
26 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8484ASTM D785
Tensile Strength 60.7 MPa8800 psiASTM D638
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %ASTM D638
Elongation at Yield 2.0 - 4.0 %2.0 - 4.0 %ASTM D638
Tensile Modulus 3.20 GPa464 ksiASTM D638
Flexural Strength 97.9 MPa14200 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiASTM D790
Izod Impact, Notched 0.190 J/cm
@Thickness 6.35 mm
0.356 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 100 °C
40.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
@Thickness 6.35 mm
165 °F
@Thickness 0.250 in
Annealed; ASTM D648
Vicat Softening Point 82.0 °C
@Load 5.10 kg
180 °F
@Load 11.2 lb
50°C/h; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
Yellow Index <= 1.0 %<= 1.0 %ASTM D1003
Transmission, Visible 92 %92 %ASTM D1003
UV Transmittance <= 87.7 %
@Wavelength 340 nm
<= 87.7 %
@Wavelength 340 nm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9349 / 319966

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.