MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Diamond Like Carbon Diamonex DLC Technical Ceramic
Categories: Ceramic

Material Notes: Superhard, conformal and low friction coating of amorphous carbon with diamond-like bonds.

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 0.00500 - 30.0 microns0.000197 - 1.18 milcoating
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction >= 0.10>= 0.10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+6 - 1.00e+12 ohm-cm1.00e+6 - 1.00e+12 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 350 - 450 °C662 - 842 °F
 
Descriptive Properties
Chemical Resistanceinert
Deposition Temperature (°C)<150
Hardness8-35 Gpa
Surface Finishidentical to substrate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BACT DLC Diamond-Like Coating
Morgan Advanced Ceramics Diamonex DLC Diamond Like Carbon Coating
Eifeler Coatings Technology CROSAL® AlCrN PVD Coating
Eifeler Coatings Technology SUCASLIDE® DLC coating
Graphite, Carbon, C

CMORF8068 / 203545

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.