MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Trinseo PULSE™ 959 ABS + Polycarbonate, 10% Glass Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes: PULSE® 959 Engineering resin is a 10% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 959 Engineering resin has been used in automotive interior trim applications.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM Data
Melt Density 1.05 g/cc0.0379 lb/in³
Water Absorption 0.15 %0.15 %
Moisture Absorption at Equilibrium 0.32 %0.32 %Humidity Absorption
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/in
Melt Flow 1.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.5 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120
Tensile Strength, Ultimate 50.4 MPa7310 psiASTM Data
Tensile Strength, Yield 48.8 MPa7080 psiASTM Data
Elongation at Break 4.0 %4.0 %ASTM Data
Elongation at Yield 3.4 %3.4 %ISO Data
Tensile Modulus 3.80 GPa551 ksiISO Data.
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM Data
 0.801 J/cm
@Temperature -50.0 °C
1.50 ft-lb/in
@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO Data, Low Temp
 9.00 J/cm²42.8 ft-lb/in²ISO Data
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO Data, Low Temp
 1.80 J/cm²8.57 ft-lb/in²ISO Data
Instrumented Impact Total Energy  5.65 J
@Temperature -30.0 °C
4.17 ft-lb
@Temperature -22.0 °F
 12.4 J
@Temperature 23.0 °C
9.15 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 57.6 µm/m-°C
@Temperature 20.0 °C
32.0 µin/in-°F
@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 2.15 J/g-°C0.514 BTU/lb-°F
Thermal Conductivity 0.228 W/m-K1.58 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FUnannealed; 127°C (261°F) annealed; ASTM Data

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® FR3305 TV PC/ABS Blend, 10% Glass Reinforced
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber
Covestro Bayblend® FR 3310 TV PC/ABS Blend, 15% Glass Reinforced
RTP Company RTP 2505 Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled

PZZDW132 / 34363

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.