MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® Terra DD G16 Nylon 1012  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: VESTAMID Terra DD-G16 is an unmodified, easy–flowing, toughness-modified PA 1012 resin for injection molding compounding. Due to its semi-crystalline morphology VESTAMID Terra DD-G16 provides an excellent chemical resistance. VESTAMID® Terra DD-G16 is a development product. VESTAMID® Terra DD is the polycondensation product of 1,10-decamethylene diamine (D) and 1,12- dodecanedioic acid (D). Because both monomers are extracted from plant oils, VESTAMID® Terra DD-G is a material that is based 100% on natural resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Water Absorption at Saturation 1.6 %ISO 62
Viscosity Number 160 cm³/gISO 307
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPaISO 527-1, ISO 527-2
Elongation at Break >= 50 %ISO 527-1, ISO 527-2
Elongation at Yield 5.0 %ISO 527-1, ISO 527-2
Tensile Modulus 1300 MPaISO 527-1, ISO 527-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1/1 eU
 NB
@Temperature -30.0 °C
ISO 179-1/1 eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 16.0 kJ/m²
@Temperature -30.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 190 °C2nd heating, DSC; ISO 11357
Vicat Softening Point 168 °C
@Load 5.10 kg
Method B; ISO 306
 188 °C
@Load 1.02 kg
Method A; ISO 306
 
Descriptive Properties
Renewable Carbon (%)100ASTM 6866

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® Terra DD16 Nylon 1012
Evonik VESTAMID® NRG 1001 PA 12
Overview of materials for Nylon 12, Extrusion/Tubing Grade
Evonik VESTAMID® Terra DD22 PA1012
Evonik VESTOSINT® 1111 natural color Polyamide 12

PEVONIK992 / 192755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.