MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure at HOC +3
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Product Description

DSM’s Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. Somos® ProtoGen resins are the first stereolithography resins to demonstrate different material properties based on machine exposure control. Based on Somos® Oxetane™ chemistry, Somos® ProtoGen 18920 offers superior chemical resistance, a wide processing latitude and excellent tolerance to a broad range of temperature and humidity, both during and after the build.

Applications

This high-temperature resistant, ABS-like photopolymer is used in solid imaging processes, such as stereolithography, to build three-dimensional parts. Somos® ProtoGen 18920 provides considerable processing latitude and is ideal for the medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accurate humidity & temperature resistant parts.

Information Provided by DSM Desotech Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. North American leaders in producing fast Rapid Prototyping and Additive Manufacturing solutions utilizing all major 3D printing systems including SLA printing technology. Free 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc
@Temperature 25.0 °C
0.0419 lb/in³
@Temperature 77.0 °F
Water Absorption 0.74 %0.74 %ASTM D570-98
Viscosity 350 cP
@Temperature 30.0 °C
350 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 86 - 8786 - 87ASTM D2240
Tensile Strength, Yield 56.1 - 56.9 MPa8140 - 8250 psiASTM D638M
Elongation at Break 5.0 - 12 %5.0 - 12 %ASTM D638M
Tensile Modulus 2.577 - 2.623 GPa373.8 - 380.4 ksiASTM D638M
Flexural Strength 85.0 - 87.0 MPa12300 - 12600 psiASTM D790M
Flexural Modulus 2.442 - 2.518 GPa354.2 - 365.2 ksiASTM D790M
Izod Impact, Notched 0.220 - 0.260 J/cm0.412 - 0.487 ft-lb/inASTM D256A
 
Descriptive Properties
AppearanceGray
Dp (mm)4.2Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)76Exposure that gives 0.254mm thickness
Ec (mJ/cm2)7Critical exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure
DSM Somos® 7120 Epoxy Photopolymer, UV Postcure
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV & Thermal Postcure
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer

PDSMT010 / 93530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.