MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Oschatz-Glas HZF 033 Type P18/6-33x2 PTFE-Impregnated Glass Filament Thread
Categories: Ceramic; Glass; Glass Fiber

Material Notes: PTFE is extremely resistant to all bases, alcohols, petrol and oils. Due to a very low coefficient of friction, PTFE has the best sliding and non-stick properties of all plastics. In addition, PTFE is non-flammable and can be exposed to high temperatures. By individually coating the glass fibers, an increase in tensile force of 10 - 20% can be achieved.

Markets include Fire protection, Technical fabrics, Automotive, Protective gear, Isolations/power plant constructions, Assembly.

Information provided by Oschatz-Glas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Loss On Ignition 14.4 - 21.6 %14.4 - 21.6 %DIN ISO 1887
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °FPTFE Coating Limit
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ISO 3344
 
Descriptive Properties
Basis MaterialEC6-33 x2DIN EN 12654
CoatingPTFE
Colorbeigecan fade on exposure to light, especially UV
Linear density of the coated yarn83 tex± 10 %, DIN EN ISO 1889
Spool formatH8-bobbins or H9-bobbins
Tensile strength> 40 NDIN EN ISO 3341

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EOSCH708 / 320689

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.