MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Monprene® OM-10240 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-10240 is a specialty thermoplastic elastomer, available in NAT, BLK and colors, designed for overmolding and co-extrusion applications like grips and anti-skid parts for consumer and industrial products. Monprene OM-10240 is a low hardness, medium density, UV stabilized, opaque grade that exhibits excellent adhesion to PC, ABS, and PC/ABS.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Adhesion; Low Hardness; Light Stabilized; Low Flow; Medium Density; Lubricated; Slip; Sunlight Resistant; UV Resistant; Without Fillers

Uses: Appliances; Bonding; Cell Phones; Dental Applications; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Rubber Replacement; Sporting Goods; Toothbrush Handles; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Multi Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  35
@Time 1.00 sec
35
@Time 0.000278 hour
Injection Molded; ASTM D2240
 40
@Time 5.00 sec
40
@Time 0.00139 hour
Injection Molded, Aged 48 hrs; ASTM D2240
 43
@Time 1.00 sec
43
@Time 0.000278 hour
Injection Molded, Aged 48 hrs; ASTM D2240
Tensile Strength at Break 4.83 MPa701 psiDie C, 20 in/min, Flow; ASTM D412
 5.18 MPa751 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  1.48 MPa
@Strain 100 %
214 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 1.61 MPa
@Strain 100 %
233 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 3.16 MPa
@Strain 300 %
459 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 3.41 MPa
@Strain 300 %
495 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 450 %450 %Die C, 20 in/min, Flow; ASTM D412
 470 %470 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 21.4 kN/m122 pliDie C, 20 in/min, Flow; ASTM D624
 21.9 kN/m125 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set  39 %
@Temperature 22.8 °C,
Time 79200 sec
39 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 80 %
@Temperature 70.0 °C,
Time 79200 sec
80 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 138 - 160 °C280 - 320 °F
Middle Barrel Temperature 182 - 199 °C360 - 390 °F
Front Barrel Temperature 182 - 199 °C360 - 390 °F
Nozzle Temperature 193 - 210 °C380 - 410 °F
Melt Temperature 177 - 199 °C350 - 390 °F
Mold Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
Drying Temperature 60.0 °C140 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® OM-10240-02 Thermoplastic Elastomer

PTEKNQ0894 / 237385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.