MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Chemlok® 6411 Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 6411 adhesive is used to bond a variety of rubber compounds to metal and plastic substrates during vulcanization. It is formulated without heavy metals and composed of a mixture of polymers and heat-reactive components dissolved or dispersed in an organic solvent system. For general use, Chemlok 6411 adhesive should be used as a covercoat adhesive over Chemlok 205 or 207 primer. Chemlok 205 or 207 primer helps to ensure environmental resistance of the bonded assembly and adhesion to the substrate. In some applications, Chemlok 6411 adhesive may be used as a one-coat adhesive. This adhesive will bond compounds based on natural rubber (NR), polyisoprene (IR), styrene-butadiene (SBR), polybutadiene (BR), polychloroprene (CR), nitrile (NBR), butyl (IIR) and EPDM polymers to most metals, alloys and rigid plastic substrates.

Features: bonds a wide variety of elastomer compounds to rigid substrates during vulcanization; can be used as a one-coat adhesive. applies easily by spray, dip, brush or roll coat methods. provides good resistance to heat, oil and corrosive-type conditions. formulated without heavy metals.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.969 - 1.01 g/cc0.0350 - 0.0364 lb/in³
Solids Content 22 - 26 %
@Temperature 130 °C,
Time 108000 sec
22 - 26 %
@Temperature 266 °F,
Time 30.0 hour
by weight, Dry residue
Brookfield Viscosity 200 - 600 cP
@Temperature 25.0 °C
200 - 600 cP
@Temperature 77.0 °F
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 25.0 °C77.0 °FSeta
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
12.0 Month
@Temperature 69.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9049 / 232438

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.