MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC SABIC® LLDPE 324CE PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE 324CE is a Linear Low Density Polyethylene natural resin typically used for wire and cable applications. SABIC® LLDPE 324CE contains a low level of antioxidants and does not contain any antiblock and/or slip agents. It also exhibits good Environmental Stress Crack Resistance (ESCR). Sufficient Cu-inhibitor should be added to meet specific ageing requirements. For jacketing applications, addition of Carbon Black or UV stabilizer is required. Applications - Telecommunication and Power cable (LV, MV, HV) jacketing. - Halogen-free flame retardant (HFFR) compounds. - One-step or two-steps silane crosslinkable for cable insulation. This product is not intended for and must not be used in any pharmaceutical/medical applications. Mechanical and electrical properties. Test specimens were prepared by compression moulding according to ASTM D 4703.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505
Melt Flow 3.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ISO 868
Tensile Strength at Break 22.0 MPa3190 psiISO 527-2
Tensile Strength, Yield 13.0 MPa1890 psiISO 527-2
Elongation at Break 1900 %1900 %ISO 527-2
Elongation at Yield 21 %21 %ISO 527-2
Flexural Modulus 0.500 GPa72.5 ksiISO 178
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.50e+15 ohm-cm8.50e+15 ohm-cmASTM D257
Dielectric Constant 2.2
@Frequency 60 Hz
2.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 30.0 kV/mm>= 762 kV/in2000 V/sec; ASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
0.00050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FSABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11062 / 244529

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.