Aliphatic, rigid polyurethane Key Properties: - Excellent physical properties after PC cure
- Free of mercury, MOCA or TDI
- Excellent U.V. stability
- Specially formulated for castings into either tin or platinum silicone molds
Applications: - For room temperature hand-batch or vacuum assisted casting methods
Cure 1: 24 hours at 77°F + 4 hours at 175°F Cure 2: 7 days at 77°F + 4 Hours at 175°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |