MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Syensqo (Solvay Specialty Polymers) Xencor™ PA66 LCF-2030 Long Glass Fiber Thermoplastic. Electrical conductive grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 66 (PA66)

Material Notes: Long Glass Fiber Thermoplastic. Electrical conductive grade. PA66/PA6 base, 30% LCF. Natural.

Xencor™ PA66 LCF-2030, a 30% long carbon fiber reinforced, heat stabilized PA66, can easily be processed on most injection molding machines.

The material exhibits an excellent combination of high stiffness and impact performances, while ensuring ease of processing and fast cycle times. It provides high strength, outstanding stiffness retention at high temperature, excellent creep and fatigue resistance, isotropic mechanical properties with low isotropic shrinkage, and excellent surface finish.

Available in natural, the pellet length is 7mm.

Natural: Xencor™ PA66 LCF-2030 NT-7

Features: Creep Resistant; Fatigue Resistant; High Stiffness; High Strength; Low Shrinkage; Outstanding Surface Finish

Injection notes: Pre-Drying
- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried. At a humidity content above 0.1%, the material will begin to degrade. Recommended drying time is 4 hours at 110°C in dry-air dryer.
Mold Temperature
- The mold temperature is a compromise between the optimum properties that can be obtained from high crystallization, and cycle time. This product can be processed at mold temperatures between 80°C and 160°C. Optimum surface quality requires a mold temperature above 100°C.
Regrind
- This product should only be recycled with special care. The regrind content must never exceed 15%, and only regrind of optimum quality should be used. In any case, part properties should be checked.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Moisture Absorption 1.70 %1.70 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0025 cm/cm0.0025 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 325 MPa47100 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 24.0 GPa3480 ksiISO 527-2
Flexural Strength 435 MPa63100 psiISO 178
Flexural Modulus 22.5 GPa3260 ksiISO 178
Charpy Impact Unnotched 5.50 J/cm²26.2 ft-lb/in²ISO 179
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 ohm100 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FISO 11359-2
Thermal Conductivity 0.510 W/m-K3.54 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 300 °C518 - 572 °F
Middle Barrel Temperature 270 - 300 °C518 - 572 °F
Front Barrel Temperature 285 - 310 °C545 - 590 °F
Nozzle Temperature 285 - 320 °C545 - 608 °F
Melt Temperature <= 310 °C<= 590 °FInjection
Mold Temperature 80.0 - 160 °C176 - 320 °F
Drying Temperature 110 °C
@Time 14400 sec
230 °F
@Time 4.00 hour
 
Descriptive Properties
AvailabilityEurope
ColorNatural Color
FormsPellets
ProcessingCompression Molding; Injection Molding; Overmolding
RoHS ComplianceYes
Suggested Max Regrind (%)15Injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4623 / 280423

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.